Oil Resistance And Low Temperature Resistance HNBR Compound Rubber For Seals
Description:
HNBR is made via selective hydrogenation of the NBR butadiene groups which improves the temperature and ozone resistance considerably. HNBR is widely known for its physical strength and retention of properties after long-term exposure to heat, oil, and chemicals. HNBR has better heat resistance; oxidation resistance; tensile strength and abrasion resistance than standard nitrile (NBR). Also an excellent choice for automotiverefrigerant service.Hydrogenated nirtrile results from the hydrogenation of standard nitrile.
Temperature range:-25℉to 300℉
Application:
Oil industry Auto car industry Aircraft industry
Compound rubber products and hydrogenated nitrile rubber plate, molding products.
Typical Properties:
FAQ:
About the type :
Customer can provide the standard grade details for we reference we will chose similar grades.
Provided the typical properties data also help us make customized HNBR rubber for you
About our production capacity :
We are able to produt 500kg/day hydrogenated nitrile
About the sample:
We would like to provide customer 0.5kg Hydrogenated nitrile butadiene rubber free sample based on your requirements, Courier charge will be collected
About the delivery time :
Standard grades can make 500kg can be prepared within 3 working days,
customzied grades delivery time must be based on the R& D schedule
About payment :
Ali insurance payment items is avaiable, TT to our company account is also ok
End Product: O ring, Gasket, Rubber packer etc.
After-sales tip
HNBR material used in very widely applications, please confirmed typical properties and chemical resistance before ask for the sample. Our bulk production formula will be same with the sample. Once anything difference with the arrangement we support third part test, if its our fault we have duty to help customer solve the problem or agree return the products.
Technical Property:
Molding HNBR Compound Data Sheet ES1270 | |||||
Press cure Sheet 170 ℃* 20 min Button 170 ℃* 30min | |||||
Post cure | 150℃*4hrs | Unit | Test Methods | Value | |
Original Properties) | |||||
Shore A hardness | - | D-2240 | 73 | ||
Tensile strength | Mpa | D-412 | 22.7 | ||
Elongation | % | D-412 | 267 | ||
Compression set 150 ℃@ 70 hrs | D-395 | 19 | |||
Aging test 150℃@ 70 hrs | |||||
Shore A Hardness change | - | D-573 | +3 | ||
Tensile strength change | % | D-573 | +8 | ||
Elongation change | % | D-573 | -1 | ||
Volume change | % | D-471 | -5 | ||
Oil resistance:IRM903#150 ℃@ 70 hrs | |||||
Shore A Hardness change | - | D-471 | -2 | ||
Tensile strength change | % | D-471 | -1.1 | ||
Elongation change | % | D-471 | -7 | ||
Volume change | % | D-471 | +10 |